Same Paint. Same Specification. Five Different Finishes.

Same Paint. Same Specification. Five Different Finishes.

MYRO

Author: MYRO

Published on: 2026-11-06

5 min read

Picture five painters working along the same corridor. They’re using the same paint, over the same primer, to the same specification. By the next morning, one section looks slightly dull, another has a band of sheen where two passes met, and the corners on a third have a heavier texture. The paint schedule is the same for every wall. What varies is how much paint each pass leaves behind.

Dry film thickness compliance starts while the paint is still wet. Catch a thin or heavy coat on the first wall and the crew can adjust before the same problem reaches the rest of the floor.

What the paint specification asks for

Wet film thickness (WFT) is the depth of the coating as applied. Dry film thickness (DFT) is the depth of the film left after drying. The product’s technical data sheet (TDS) may give a recommended range per coat. The project specification sets out what the team has to deliver and how it will be accepted.

For example, Jotun’s Fenomastic My Home Smooth Silk data sheet gives typical ranges of 88 to 150 microns wet and 35 to 60 microns dry per coat. On a coating with 40% solids by volume as applied, a 100-micron wet film would give an estimated 40-micron dry film. Permitted thinning changes that estimate, so check the data sheet and approved application method before setting a wet-film target. Jotun technical data sheet · ASTM guidance on wet film measurement

How five painters leave five different films

A painter may reload the roller halfway up a wall, slow down around a door frame, or overlap a section that has already started to dry. With a spray gun, changes in travel speed, tip condition, overlap or distance from the wall can also change how much paint lands in a given area. Each adjustment is small. The difference becomes visible when you stand back and look down the corridor.

A thin coat can leave the base showing through or dry to a different sheen. A heavy coat uses more paint per square metre and can crack as it dries, especially where material builds up in corners. Porous repairs can also leave dull patches, which is why the crew needs to check the primer and surface preparation before treating a patch as a thickness issue. Sherwin-Williams guidance on uneven gloss · Sherwin-Williams guidance on mudcracking

How to verify paint film thickness on site

  1. Start with an approved mock-up. Use the specified substrate, primer and topcoat. Agree on the target for each coat and confirm whether acceptance covers the topcoat or the full coating system.
  2. Check the first passes while they’re wet. Where the project’s test method allows, a wet-film comb gives a quick estimate. Log the readings with the wall location, coat and batch so the crew can trace any adjustment.
  3. Verify the dry film where the specification calls for it. Use a method suited to the surface and coating system. On drywall, a suitable ultrasonic gauge can measure the coating, but a reading may include both primer and topcoat. Confirm which layers the method can resolve before comparing readings with a per-coat target. DeFelsko guidance on measuring paint on drywall

Say the first spray pass on a trial wall reads within range and the readings where passes overlap are above the target. Check the spacing and pace of the passes, adjust the setup and measure both areas again on a fresh section. Once the crew has a result it can repeat, record the settings alongside the readings.

That record is useful at a shift change. The next operator can see which mix and spray setup produced the approved finish, which locations were checked and where the earlier pass ran heavy. If the next floor uses a different coating, the crew knows which assumptions to revisit before it starts.

What to check once production starts

The first approved wall gives the foreman a reference for the rest of the floor. Put the agreed checks into the work sequence so the crew knows which walls to sample and when to pause after a change in setup. Pay particular attention to transitions the mock-up might not have represented, such as a long wall that breaks into narrow sections around doors. Those sections are easy to walk past during a routine coverage check.

If a reading falls outside the agreed range, mark the location and check the nearby passes before deciding how much of the wall needs attention. A heavy strip by one opening calls for a closer look at how that section was painted. Similar readings across several walls call for a review of the shared setup. Recording where the pattern begins and ends gives the next shift something specific to verify.

Where MYRO helps crews repeat the approved finish

With MYRO, the spray setup gives the operator a repeatable starting point for pass speed, pressure and distance from the wall. The team can run a trial area, check the wet film and adjust the setup before repeating it on comparable walls. If the coating or substrate changes, the next trial gives the operator a chance to check the settings again. How MYRO controls spray application

The finish still has to look right under the building’s lighting. That check can catch lap marks and flashing during the handover walk, while the film measurements give the team a record of what was applied. For a contractor finishing several floors in sequence, the value is being able to trace the approved wall back to a setup the next crew can repeat.

Talk to MYRO about trialling your specified coating on site.

Share

Company Logo

Singapore Headquarters

111 North Bridge Road
#07-11 Peninsula Plaza Singapore (179098)

Dubai Branch

7, 599- Jebel Ali Industrial First
Dubai, UAE- 507187

Contact Number: +971 54 995 4416
Email [email protected]


© All Rights Reserved MYRO International PTE 2026